Cheapest Per Kg Is Not Cheapest Per Part: How to Compare Plastic Dana Quotes
Compare plastic dana quotes by the material cost of each good part, not by the rate per kg. Two quotes for the same grade name can give different part weights and different reject rates on your machine, and either one can turn the lower rate into the higher cost per part.
Why is the rate per kg not enough?
You buy by the kilo but sell by the piece. Between the two sit what the rate includes, what each part weighs and how many parts you reject. Our guide to what sets the plastic raw material price explains the first: compare the landed cost per kg, with rate, GST and freight together, and only like grade against like grade. This method takes that figure on to the part.
What is the formula for cost per good part?
Cost per good part = landed cost per kg × shot weight in kg ÷ (1 − rejection rate)
- Landed cost per kg: the quoted rate plus freight, with GST treated the same way on every quote.
- Shot weight: shot volume in cm³ × density in g/cm³, divided by 1,000 to give kg. Include the runner if you do not regrind it.
- Rejection rate: rejected parts over total parts moulded, so 4% is 0.04.
Estimate shot weight from the density on each test report, then replace it with the weight you measure on the trial.
Why does density change what you pay per part?
Your mould fixes the volume of the part, not its weight, which is volume times density. Polypropylene is a light polymer, at roughly 0.90 to 0.91 g/cm³, and a reading well above that band suggests other polymers or mineral filler in the material. A denser dana fills the same cavity with more kilos, which can cancel a lower rate before any part is rejected. See how to read a granule test report.
How does the rejection rate change the cost?
Every rejected part used material you paid for. Dividing by (1 − rejection rate) spreads that loss across the parts you can sell: at 2% rejects you divide by 0.98, at 6% by 0.94. Take the rate from a fair trial on the same mould and the same settings, as set out in our guide to trialling a new dana supplier. Regrinding rejects recovers some material, but not the machine time, power and labour. A melt flow index that wanders between batches also moves cycle time and part weight.
What does a worked example look like?
The figures below are hypothetical and chosen only to show the method. They are not our prices or any supplier's. The rate is shown as an index, with Quote A set at 100.
| Line | Quote A (example) | Quote B (example) |
|---|---|---|
| Rate per kg, as an index | 100 | 95 |
| Density on the test report | 0.91 g/cm³ | 0.97 g/cm³ |
| Shot volume, same mould | 220 cm³ | 220 cm³ |
| Shot weight | 200.2 g | 213.4 g |
| Rejection rate on trial | 2% | 6% |
| Material per good part (index) | 20.43 | 21.57 |
In this example Quote B is 5% cheaper per kg but about 5.6% dearer per good part.
What should your quote comparison sheet look like?
Give each quote its own column. Leave a cell empty rather than guess: an empty cell is a question for the supplier.
| Line | Quote A | Quote B | Quote C |
|---|---|---|---|
| Supplier, grade and shade | |||
| Quoted rate per kg | |||
| GST and freight included? | |||
| Landed cost per kg | |||
| MFI on the test report | |||
| Density on the test report | |||
| Moisture on the test report | |||
| Shot weight measured on trial (g) | |||
| Rejection rate on trial (%) | |||
| Cost per good part |
How can Markandey Polymers help you compare?
We manufacture PP and PPCP granules at our own unit in Narela, Delhi, and every batch is tested in our in-house lab for MFI, density, moisture, contamination, elongation and Izod impact strength before dispatch. See how we test. We quote on the day rather than publish a fixed price list. Tell us the part, the process and the shade, and ask for a sample to fill in our column.